Polyurethane springs for compression, die and damping applications
In a die, a steel spring offers long travel and predictable force, but it can break without warning. A polyurethane spring delivers more force in less space and does not shatter into fragments, at the cost of a shorter stroke.
Key takeaways
- A polyurethane spring is an elastomer element that compresses under load, then returns to its shape when the load is removed.
- It delivers high force in a compact envelope, absorbs part of the energy and operates without metallic noise.
- Its force-deflection curve is not linear and depends as much on geometry and confinement as on hardness.
- It differs from a steel spring in its shorter stroke, its shock tolerance and the absence of sudden fracture.
In a die, a steel spring offers long travel and predictable force, but it can break without warning. A polyurethane spring delivers more force in less space and does not shatter into fragments, at the cost of a shorter stroke.
Between these two options, the right choice depends on the available travel, the cycle rate and the space around the part. Hardness alone cannot settle the question.
Before replacing a spring, it is therefore worth understanding how an elastomer generates its force and what limits its service life.
How a polyurethane spring works
Polyurethane is a nearly incompressible elastomer. When it is compressed, its volume stays roughly constant, which forces it to bulge sideways. That bulging is what creates the return force.
This characteristic has two practical consequences. First, the part needs space around it to deform. Second, the force rises faster and faster as compression increases, unlike a steel spring, whose response is nearly linear.
Hardness, geometry and confinement
Hardness influences stiffness, but it is not enough to define behavior. A ring-shaped part, a solid cylinder or a custom shape of the same hardness will produce very different force curves.
Confinement matters just as much. A polyurethane compression spring housed in a tight bore stiffens as soon as it touches the wall. That is why the page on polyurethane compression springs emphasizes a full study of the assembly rather than a simple dimensional match.
Polyurethane die springs in tooling
In stamping, punching and bending dies, the spring is used to return a blank holder, eject a part or strip a punch. Polyurethane die springs fill this role in many shops.
Steel die springs are covered by the ISO 10243 standard on compression springs for press tools, which classifies their stiffness into four color-coded categories. Polyurethane does not follow this system. Its force is defined by the stroke, the preload and the geometry specific to each assembly.
A polyurethane spring offers several advantages in a die. It develops high force in a confined volume, tolerates repeated impact well and does not break into metal fragments that could damage the tool. Its stroke, however, remains shorter than that of a coil spring.
Urethane spring pads and damping
The urethane spring pad sits on the boundary between a spring and a bumper. It cushions the end of a stroke, protects a cylinder or softens the return of a mechanism. Unlike a bumper, which reacts mainly on contact, the spring works over its entire stroke. The page on custom polyurethane bumpers covers the other side of these applications.
Energy return and damping
A steel spring returns almost all the energy it stores. Polyurethane dissipates part of it as heat with each cycle. This hysteresis is an advantage when you need to calm a rebound or absorb a shock.
It becomes a limitation at high cycle rates. If cycles follow one another too quickly, heat builds up in the core of the part, stiffness drops and service life shortens. Cycle rate, dwell times and ambient temperature should therefore be part of the specification.
A spring that breaks or loses force too quickly often points to a stroke, cycle rate or confinement that was poorly assessed. Those three data points are enough to start studying the assembly. Have your assembly reviewed
Steel, rubber or polyurethane springs
| Criterion | Steel spring | Rubber elastomer | Cast polyurethane |
|---|---|---|---|
| Force in a small volume | Moderate | Low to moderate | High |
| Available stroke | Long | Short | Short |
| Force-deflection curve | Nearly linear | Progressive | Progressive |
| Damping | Very low | Good | Good |
| Failure mode | Often sudden fracture | Tearing, deformation | Wear, compression set |
| Oil resistance | Good | Poor for natural rubber | Good |
| High temperature | Very good | Good depending on compound | Limited to about 80 °C |
| Noise | Possible on contact | Low | Low |
Replacing a metal spring with polyurethane makes sense when space is limited, impacts are frequent or a fracture poses a risk to the tool. It makes less sense when the stroke is long, the cycle rate very high or the temperature above about 80 °C.
Compared with rubber, polyurethane carries more load for the same volume and better resists oil and abrasion. The article on choosing between polyurethane and rubber details these differences.
Specifying an industrial polyurethane spring
Compression set, meaning the portion of compression that is not recovered after a sustained load, is one of the most important criteria. The ASTM D395 standard on compression set is the reference used to measure it.
There is no universal allowable compression percentage. A load-deflection curve can, however, be established, provided the measurement conditions and acceptance criteria are agreed in advance. For an industrial polyurethane spring, the following information is essential.
- The envelope, meaning the free height, diameter, bore and available lateral space
- The stroke, including the preload, normal stroke and maximum stroke
- The force required at specific deflections
- The cycles, meaning the cycle rate, dwell times and hours of service
- The environment, including temperature, lubricants and cutting fluids
The polyurethane Shore hardness chart helps pinpoint the starting range, which is then validated by testing.
When to choose a polyurethane spring over a steel spring
The polyurethane spring is the clear choice when space is tight, impacts are frequent or a fracture would put the tool at risk. The steel spring remains preferable for long strokes, very high cycle rates and temperatures above about 80 °C.
Its performance, however, depends on a complete study that accounts for geometry, confinement, stroke, cycle rate and temperature. OEM equipment manufacturers benefit from building these parameters in from the design stage.
To design a custom compression element, share your drawing, target stroke and required force.
FAQ
What is the service life of a polyurethane spring?
The service life of a polyurethane spring depends on the required stroke, the cycle rate, dwell times under load, temperature and the space available for deformation. Excessive compression or too fast a cycle rate heats the part and accelerates compression set. A test on the actual assembly, with a measured load-deflection curve, makes it possible to validate service life.
Can a steel spring be replaced with a polyurethane spring?
Often, but not by simply copying the dimensions of the original part. Polyurethane offers a shorter stroke and a progressive response, and it needs room to bulge sideways. The replacement must therefore start from the force required at each point in the stroke, the available envelope and the cycle rate. A study of the assembly confirms feasibility before series production.
Why does a polyurethane spring lose force?
A loss of force generally comes from compression set, meaning the portion of compression that is no longer recovered. It increases when the part stays compressed for long periods, operates at high temperature or exceeds the intended compression. Too fast a cycle rate also promotes internal heat buildup. Revising the geometry, hardness, confinement or formulation corrects this behavior in repetitive applications.